【大学化学】doi: 10.3866/PKU.DXHX202312021
“荧光海”是指在夜晚或黑暗环境中,海水表面发蓝光的景象,又称“蓝眼泪”。本科普实验着眼于引导人们了解该有趣自然现象,探究背后的科学原理,以智能缓释材料海藻多糖水凝胶包埋发光原料,根据化学发光能量转移原理制备可持续发光的多彩藻胶球,并基于此推出一种便携科普实验盒,可随时随地重现属于自己的澎湃“蓝眼泪”。本科普实验将糖化学、光化学和材料化学知识应用于自然现象的解读与应用,向公众充分展现浪漫美妙的化学科学。
【无机化学学报】doi: 10.11862/CJIC.20240255
采用原位聚合法制备了氯氧化铋(BiOCl)与聚苯胺(PANI)复合的Ⅱ型异质结光催化剂BiOCl/PANI,并采用X射线衍射(XRD)、傅里叶变换红外光谱(FTIR)、透射电子显微镜(TEM)、X射线光电子能谱(XPS)、紫外可见漫反射光谱(UV-Vis DRS)和N2吸附-脱附测试等多种技术手段对其进行了表征,考察了BiOCl/PANI在模拟可见光下对罗丹明B (RhB)的光催化降解性能。实验结果表明:BiOCl/PANI催化剂比PANI和BiOCl具有更高的光催化活性,在RhB质量浓度为50 mg·L-1、PANI与BiOCl的物质的量之比为0.02∶1、50 mg·L-1的催化剂条件下,所制备的BiOCl/PANI光催化150 min后,RhB降解率为98.8%,速率常数为0.031 min-1;经过4次循环实验后,RhB降解率从98.8%降低至98.4%,表现出良好的稳定性和可重复利用性。光催化剂BiOCl/PANI实现了电子和空穴对的快速分离,降低了二者在催化剂内部的复合速率,提高了光催化性能。
【大学化学】doi: 10.12461/PKU.DXHX202405147
仪器分析实验“分子荧光法测定罗丹明B的含量”存在实验过于简单、未考虑实际情况等问题。因此,本改进实验在三维荧光扫描模式下获取样本数据,不进行复杂预处理,而是运用化学计量学算法解析出目标分析物的纯信号,进而实现了染色辣椒中罗丹明6G和123的同时测定。本改进实验提高了学生全面考虑问题和创新解决问题的能力。
【无机化学学报】doi: 10.11862/CJIC.20240428
通过微波加热方式,快速合成了3个葡萄糖修饰的双席夫碱。通过比浊度分析、HRP/Amplex Red实验、DCFH-DA荧光探针实验、NBT分析法以及MTT实验检测它们抑制金属离子诱导的Aβ聚集、减少活性氧(ROS)生成及抑制Aβ聚集产生的细胞毒性。发现葡萄糖修饰的双席夫碱都能有效抑制金属离子(Zn2+、Cu2+)诱导的Aβ1~40的聚集,降低Cu2+-Aβ加合物催化产生ROS水平、提高Cu2+-Aβ作用的细胞内超氧化物歧化酶的活力,有效抑制Zn2+或Cu2+诱导Aβ聚集而产生的神经细胞毒性并大幅提高细胞存活率。作为对比,我们也检测了相同条件下的氯碘羟喹(cliquinol, CQ)和没有葡萄糖修饰的同类双席夫碱的活性,发现葡萄糖修饰的双席夫碱各方面活性均好于CQ;葡萄糖修饰的双席夫碱自身毒性小、抗氧化和提高Aβ与金属离子共同处理的细胞的存活率方面均优于未葡萄糖官能化的同类双席夫碱。
【无机化学学报】doi: 10.11862/CJIC.20240219
A simple two-step hydrothermal method synthesized four different CdS/Fe3O4 photocatalysts with varying ratios of mass of CdS to Fe3O4. The composition and morphology of the prepared samples were investigated using X-ray diffraction (XRD), Raman spectrum, X-ray photoelectron spectroscopy (XPS), scanning electron microscopy (SEM), and transmission electron microscopy (TEM). Solid UV reflectance spectra testing found that CdS/Fe3O4 nanocomposites had good light absorption throughout the spectral range, promoting their photocatalytic properties. Under visible light irradiation, CdS/Fe3O4 (2:5) with a mass ratio of 2:5 exhibited excellent photocatalytic performance, with a degradation rate of 98.8% for rhodamine B. Furthermore, after five cycles of photocatalytic degradation reaction, the rhodamine B degradation rate remained at 96.2%, indicating that the photocatalysts have good photocatalytic stability.
【无机化学学报】doi: 10.11862/CJIC.20250028
A flower-like BiOBr photocatalyst (CS/BiOBr) was prepared by using the carbon material derived from corn straw (CS) as the carrier. The prepared composites were characterized by X - ray diffraction (XRD), Fourier transform infrared (FIIR) spectra, scanning electron microscope (SEM), X - ray photoelectron spectra (XPS), and UV-Vis diffuse reflectance spectra (UV-Vis DRS). The SEM analyses indicate that the introduction of CS promotes the formation of a unique flower-like structure in BiOBr, which not only optimizes the efficiency of light capture but also increases the specific surface area of BiOBr. The bandgap of the composite was narrower compared with the pure BiOBr. The CS/BiOBr composites exhibited higher photocatalytic activity than pure CS and BiOBr under visible light irradiation, and a higher first-order reaction rate constant (k) of 0.043 7 min-1 than BiOBr (0.014 6 min-1), and exhibited excellent stability and reusability during the cyclic run. The enhanced photocatalytic activity is attributed to the efficient separation of photoinduced electrons and holes. Superoxide radicals and holes were the major active species.
【物理化学学报】doi: 10.3866/PKU.WHXB202307024
梯形共轭聚合物(CLPs)因其独特的光电性质而受到广泛关注。绝大多数CLPs是通过溶液方法合成的,但近年来,在超高真空环境中进行的表面原位合成策略逐渐崭露头角,成为CPL合成的新方法。表面原位合成方法能够克服传统溶液合成的限制,如随着聚合度增加而受限的溶解度和结构稳定性,从而实现复杂共轭结构的精确合成。Azulene衍生物是在表面合成非苯型CLPs的有吸引力的前体。与传统的只含六元环的CLPs相比,使用烷基取代的azulene作为前体分子,有望获得具有复杂骨架结构的CLPs,从而调控其电子性质,但目前很少有人探索这种策略。本文报道了3,3'-二溴-2,2’-二甲基-1,1’-联薁(DBMA)在Au(111)表面上的热化学反应。在室温的Au(111)衬底上,我们发现沉积的分子在重构表面的fcc (面心立方堆积)区域形成无定型的聚集体,并在100 ℃以下保持形貌不变。当退火温度高于150 ℃后,DBMA发生脱溴反应并与金原子络合形成具有复杂空间立体结构的2,2’-二甲基-1,1’-联薁有机金属聚合物,并展现出迥异的图像特征。随后在更高温度下退火,有机金属聚合物脱去金属原子并经历碳碳偶联反应。该过程伴随着甲基与相邻薁单元之间的分子内环化反应,形成了含有benzo[a]azulene单元的梯形共轭聚合物。有趣的是,我们发现当一侧甲基参与反应并在聚合物中形成六元环时,会显著地弯折聚合物链,使得另一侧甲基与薁单元之间的距离增加,并抑制预期的环化过程。我们通过键分辨扫描探针显微镜对反应过程中的相关结构进行了研究,发现反应结果与反应中间结构的应力关联紧密。我们的结果表明,烷基取代的azulene前体可应用于非苯型碳纳米结构的表面合成,并有望实现扩展的非苯型二维碳纳米结构。
【物理化学学报】doi: 10.3866/PKU.WHXB202309011
催组装是用于描述催组剂帮助下的分子组装的新概念,目前还未报道过催组装过程的分子水平表征。本文中,我们利用扫描隧道显微镜(STM),在辛酸和高序热解石墨之间的液固界面,观察到了1, 3, 5-三(4-羧基苯基)-苯(BTB)亚稳态自组装网格在主客体识别过程中的催组装过程。实验中采用的是低浓度的客体分子酞菁铜(CuPc),以及晕苯(COR)分子。我们对比了单客体(COR/BTB或CuPc/BTB)体系和多客体(COR & CuPc/BTB)体系中客体分子在主客体组装过程中的不同吸附特征。在多客体分子(COR & CuPc/BTB)体系中,晕苯分子优先填入主体六边形网络中,随着组装的进行逐渐被酞菁铜分子取代。晕苯分子在组装过程中发挥了催组装剂的作用,帮助低浓度酞菁铜完成了其本身无法形成的、大面积的CuPc/BTB共组装。这是首次在分子尺度观察到的完整的催组装过程,有助于指导构建更高复杂度的二维分子组装单层膜。