SYNTHESIS OF A SILICON-CONTAINING FLAME RETARDANT AND ITS SYNERGISTIC EFFECT WITH POTASSIUM-4-(PHENYLSULFONYL)BENZENESULFONATE (KSS) IN POLYCARBONATE (PC)

Dan-dan Yuan Xu-fu Cai

Citation:  Dan-dan Yuan, Xu-fu Cai. SYNTHESIS OF A SILICON-CONTAINING FLAME RETARDANT AND ITS SYNERGISTIC EFFECT WITH POTASSIUM-4-(PHENYLSULFONYL)BENZENESULFONATE (KSS) IN POLYCARBONATE (PC)[J]. Chinese Journal of Polymer Science, 2013, 31(10): 1352-1358. doi: 10.1007/s10118-013-1306-8 shu

SYNTHESIS OF A SILICON-CONTAINING FLAME RETARDANT AND ITS SYNERGISTIC EFFECT WITH POTASSIUM-4-(PHENYLSULFONYL)BENZENESULFONATE (KSS) IN POLYCARBONATE (PC)

    通讯作者: Xu-fu Cai,
摘要: A novel flame retardant (DAPSiO), containing silicon and nitrogen, was synthesized by using dichlorodiphenylsilane, -chloropropyl methyl dimethoxysilane and 1, 2-ethanediamine. DAPSiO was used together with potassium-4-(phenylsulfonyl)benzenesulfonate (KSS) to prepare a flame-retardant system for polycarbonate (PC). The structure of DAPSiO was characterized by Fourier transform infrared spectroscopy (FTIR), and 1H-NMR tests. Flammability and thermal behaviors of PC/KSS/DAPSiO systems were estimated by limited oxygen index (LOI), vertical burning test (UL-94) and thermogravimetric analysis (TGA) tests. The results showed that the flame retardancy and thermal stability of PC/KSS system were improved with the addition of DAPSiO. When 1 wt% DAPSiO and 0.5 wt% KSS were incorporated, the LOI value of PC was found to be 44, and class V-0 of UL-94 test was passed. The scanning electron microscopy (SEM) and FTIR indicated that PC/KSS/DAPSiO system held a more cohesive and denser char structure when compared with pure PC and PC/KSS system.

English


    1. [1]

      Levchik, S.V. and Weil, E[J].D., Polym. Int.2005, 54:981-[2]Deng, Y. and Wang, Y.Z. Chinese Journal of Polymer Science, 2008, 26(3):299[3]Li, X.G. and Huang, M[J].R., Polym. Int.1999, 48:387-3.0.CO;2-S' target='_blank'>[4]Vladimir, Z. and Ludmila, E[J]., Chinese Journal of Polymer Science.2008, 26 (5):553-[5]Zaikov, G.E. and Lomakin, S[J].M., J. Appl. Polym. Sci.1998, 68:715-3.0.CO;2-R' target='_blank'>[6]Lu, S.Y. and Hamerton, I[J]., Prog. Polym. Sci.2002, 27:1661-[7]Chen, X.L., Hu, Y. and Song, L., Polym. Eng. Sci., 2008, 48:116[8]Zhong, H.F., Wei, P. and Jiang, P.K., J. Polym. Sci. B:Polym. Phys., 2007, 45:1542[9]Masatoshi, I. and Shin, S[J].Polym. Adv. Technol.1998, 9:593-3.0.CO;2-U' target='_blank'>[10]Zhong, H.F., Wei, P. and Jiang, P.K., Fire Mater., 2007, 31:411[11]Liu, S.M., Lang, X[J].M. andYe, H., Eur. Polym. J.2005, 41:996-[12]Nishihara, H., Suda, Y.and Sakuma, T., J .Fire Sci., 2003, 21:451[13]Babrauskas, V., Fire Mater[J]..1995, 19:243-[14]Periadurai, T., Vijayakumarb, C[J].T. and Balasubramanian, M.J., Anal. Appl. Pyrol.2010, 89:244-[15]He, Q.L., Song, L., Hu, Y. and Zhou, S.J. Mater. Sci. 2009, 5:1308[16]Song, L., He, Q.L., Hu, Y. and Chen, H., Polym. Degrad. Stabil. 2008, 93 :627[17]Takashi, K. and John, R[J].S., J .Appl. Polym. Sci.2003, 87:1541-[18]Babrauskas, V. and Peacock, R[J].D., Fire Safety J.1992, 18:255-[19]Zhong, H.F., Wu, D. and Wei, P.J., Mater. Sci., 2007, 42: 10106

  • 加载中
计量
  • PDF下载量:  0
  • 文章访问数:  1025
  • HTML全文浏览量:  29
文章相关
  • 发布日期:  2013-10-05
  • 收稿日期:  2012-10-08
  • 修回日期:  2013-01-14
通讯作者: 陈斌, bchen63@163.com
  • 1. 

    沈阳化工大学材料科学与工程学院 沈阳 110142

  1. 本站搜索
  2. 百度学术搜索
  3. 万方数据库搜索
  4. CNKI搜索

/

返回文章