Citation: ZHAO Tian-qi, GAO Qiang, LI He-jian, XU Xiu-feng. Catalytic decomposition of N2O over Y-Co3O4 composite oxides prepared by one-step hydrothermal method[J]. Journal of Fuel Chemistry and Technology, ;2019, 47(4): 446-454. shu

Catalytic decomposition of N2O over Y-Co3O4 composite oxides prepared by one-step hydrothermal method

  • Corresponding author: XU Xiu-feng, xxf@ytu.edu.cn
  • Received Date: 8 January 2019
    Revised Date: 3 March 2019

    Fund Project: The project was supported by Shandong Natural Science Foundation (ZR2017MB020) and Graduate Innovation Foundation of Yantai University (YDYB1909)Shandong Natural Science Foundation ZR2017MB020Graduate Innovation Foundation of Yantai University YDYB1909

Figures(12)

  • Y-Co3O4 catalysts with Y/Co molar ratio of 0.03 were prepared by several methods, such as one-step hydrothermal, two-step hydrothermal, and impregnation methods, to catalyze the decomposition of N2O. Among these catalysts, the one prepared by one-step hydrothermal method exhibited the highest activity, and then the Y-Co3O4 catalysts with various molar ratios of Y/Co were synthesized by one-step hydrothermal method. Subsequently, the optimized 0.03Y-Co3O4 was impregnated by K2CO3 solution to prepare K-modified catalyst and named as 0.02K/0.03Y-Co3O4. These catalysts were characterized by X-ray diffraction (XRD), nitrogen physisorption, hydrogen temperature-programmed reduction (H2-TPR), oxygen temperature-programmed desorption (O2-TPD), scanning electron microscopy (SEM), and X-ray photoelectron spectroscopy (XPS) techniques. The results show that both Co3O4 and Y-Co3O4 exhibit spinel structure, however Y-doped Co3O4 catalysts are more active than bare Co3O4. After further modified by potassium, the 0.02K/0.03Y-Co3O4 reveals higher activity due to the more active sites (Co2+) and easier desorption of surface oxygen species than un-modified 0.03Y-Co3O4. In detail, the temperatures of N2O full conversion over 0.02K/0.03Y-Co3O4 catalyst are 325, 350, 375℃, under the reaction atmospheres of 1%N2O+Ar, 1%N2O+2%O2+Ar, 1%N2O+2%O2+8.2%H2O+Ar, respectively. In addition, over 90% conversion of N2O can be maintained at 350℃ after continuous reaction for 50 h in the co-presence of oxygen and steam on K-modified Y-Co3O4 catalyst. There is a dynamic compensation effect between apparent activation energy (Ea) and pre-exponential factor (A) in N2O decomposition over Y-Co3O4 and K-modified catalysts.
  • 加载中
    1. [1]

      REILLY J, PRINN R, HARNISCH J, FITZMAURICE J, JACOBY H, KICKLIGHTER D, MELILLO J, STONE P, SOKOLOV A, WANG C. Multi-gas assessment of the Kyoto Protocol[J]. Nature, 1999,401:549-555. doi: 10.1038/44069

    2. [2]

      ZHENG L, LI H J, XU X F. Catalytic decomposition of N2O over Mg-Co composite oxides hydrothermally prepared by using carbon sphere as template[J]. J Fuel Chem Technol, 2018,46(5):569-577. doi: 10.1016/S1872-5813(18)30024-0

    3. [3]

      YAN L, REN T, WANG X L, JI D, SUO J S. Catalytic decomposition of N2O over MxCo1-xCo2O4(M=Ni, Mg) spinel oxides[J]. Appl Catal B:Environ, 2003,45(2):85-90. doi: 10.1016/S0926-3373(03)00174-7

    4. [4]

      IVANOVA Y A, SUTORMINA E F, ISUPOVA L A, ROGOV V A. Effect of the composition of NixCo3-xO4(x =0-0.9) oxides on their catalytic activity in the low-temperature reaction of N2O decomposition[J]. Kinet Catal, 2018,59(3):365-370.

    5. [5]

      DOU Z, ZHANG H J, PAN Y F, XU X F. Catalytic decomposition of N2O over potassium-modified Cu-Co spinel oxides[J]. J Fuel Chem Technol, 2014,42(2):238-245. doi: 10.1016/S1872-5813(14)60016-5

    6. [6]

      FRANKEN T, PALKOVITS R. Investigation of potassium doped mixed spinels CuxCo3-xO4 as catalysts for an efficient N2O decomposition in real reaction conditions[J]. Appl Catal B:Environ, 2015,176/177(298)305.  

    7. [7]

      WANG Y Z, HUO X B, ZHANG K, WEI X H, ZHAO Y X. Effect of SnO2 on the structure and catalytic performance of Co3O4 for N2O decomposition[J]. Catal Commun, 2018,111:70-74. doi: 10.1016/j.catcom.2018.04.004

    8. [8]

      TURSUN M, WANG X P, ZHANG F, YU H B. Bi-Co3O4 catalyzing N2O decomposition with strong resistance to CO2[J]. Catal Commun, 2015,65:1-5. doi: 10.1016/j.catcom.2015.02.013

    9. [9]

      YU H B, TURSUN M, WANG X P, WU X X. Pb0.04Co catalyst for N2O decomposition in presence of impurity gases[J]. Appl Catal B:Environ, 2016,185:110-118. doi: 10.1016/j.apcatb.2015.12.011

    10. [10]

      YU H B, WANG X P, WU X X, CHEN Y. Promotion of Ag for Co3O4 catalyzing N2O decomposition under simulated real reaction conditions[J]. Chem Eng J, 2018,334:800-806. doi: 10.1016/j.cej.2017.10.079

    11. [11]

      KIM M J, LEE S J, RYU I S, JEON M W, MOON S H, ROH H S, JEON S G. Catalytic decomposition of N2O over cobalt based spinel oxides:The role of additives[J]. Mol Catal, 2017,422:202-207.

    12. [12]

      XUE L, HE H, LIU C, ZHANG C B, ZHANG B. Promotion effects and mechanism of alkali metals and alkaline earth metals on cobalt-cerium composite oxide catalysts for N2O decomposition[J]. Environ Sci Technol, 2009,43(3):890-895. doi: 10.1021/es801867y

    13. [13]

      DZIEMBAJR, ZAITZ, RUTKOWSKAM, MOLENDAM, CHMIELARZL. Nanostructured Co-Ce-O systems for catalytic decomposition of N2O[J]. Catal Today, 2012,191(1):121-124. doi: 10.1016/j.cattod.2012.02.045

    14. [14]

      YOU Y, CHANG H, MA L, GUO L, QIN X, LI J Y, LI J H. Enhancement of N2O decomposition performance by N2O pretreatment over Ce-Co-O catalyst[J]. Chem Eng J, 2018,347:184-192. doi: 10.1016/j.cej.2018.04.081

    15. [15]

      ABUZIED B M, BAWAKED S M, KOSA S A, SCHWIEGER W. Effect of Pr, Sm, and Tb doping on the morphology, crystallite size, and N2O decomposition activity of Co3O4 nanorods[J]. J Nanomater, 2015,56(12):1417-1423.  

    16. [16]

      GRANGER P, ESTEVES P, KIEGER S, NAVASCUES L, LECLERCQ G. Effect of yttrium on the performances of zirconia based catalysts for the decomposition of N2O at high temperature[J]. Appl Catal B:Environ, 2006,62:236-243. doi: 10.1016/j.apcatb.2005.07.015

    17. [17]

      ABU-ZIED B M, BAWAKED S M, KOSA S A, ALI T T, SCHWIEGER W, AQLAN F M. Effects of Nd-, Pr-, Tb-and Y-doping on the structural, textural, electrical and N2O decomposition activity of mesoporous NiO nanoparticles[J]. Appl Surf Sci, 2017,419:399-408.  

    18. [18]

      ABU-ZIED B M, BAWAKED S M, KOSA S A, SCHWIEGER W. Impact of Gd-, La-, Nd-and Y-doping on the textural, electrical conductivity and N2O decomposition activity of CuO catalyst[J]. Int J Electrochem Sci, 2016,11:2230-2246.

    19. [19]

      QIU Y J, HUANG S Q, PANG Z T, SONG Y J, WANG X C, LI C Q, WANG H. Catalytic decomposition of N2O over CuYO/γ-Al2O3 catalysts[J]. Environ Chem, 2018,37(7):1591-1598.  

    20. [20]

      LIU Z M, HE C X, CHEN B H, LIU H Y. CuO-CeO2 mixed oxide catalyst for the catalytic decomposition of N2O in the presence of oxygen[J]. Catal Today, 2017,297:78-83. doi: 10.1016/j.cattod.2017.05.074

    21. [21]

      PAN Y F, FENG M, CUI X, XU X F. Catalytic activity of alkali metal doped Cu-Al mixed oxides for N2O decomposition in the presence of oxygen[J]. J Fuel Chem Technol, 2012,40(5):601-607. doi: 10.1016/S1872-5813(12)60024-3

    22. [22]

      STELMACHOWSKI P, MANIAK G, KOTARBA A, SOJKA Z. Strong electronic promotion of Co3O4 towards N2O decomposition by surface alkali dopants[J]. Catal Commun, 2009,10(7):1062-1065. doi: 10.1016/j.catcom.2008.12.057

    23. [23]

      LI H J, ZHENG L, ZHAO T Q, XU X F. Effect of preparation parameters on the catalytic performance of hydrothermally synthesized Co3O4 in the decomposition of N2O[J]. J Fuel Chem Technol, 2018,46(6):717-724. doi: 10.1016/S1872-5813(18)30031-8

  • 加载中
    1. [1]

      Yingxue Lu , Ying Xin , Hao Wu , Jin Wang , Zhaoliang Zhang . Recent progress in catalysts for direct catalytic decomposition of N2O. Chinese Chemical Letters, 2026, 37(10): 112555-. doi: 10.1016/j.cclet.2026.112555

    2. [2]

      Yuanjun LIU , Jiayang JIANG , Rui WANG , Jiangnan HU , Chaoyi YUAN , Xingmei GUO , Junhao ZHANG , Guoxing ZHU . Crystallinity and oxidation degree tuning of Ru for alkaline hydrogen oxidation. Chinese Journal of Inorganic Chemistry, 2026, 42(9): 1933-1944. doi: 10.11862/CJIC.20250373

    3. [3]

      Guangnan SHAN , Yuhui WANG , Yueru WU . Preparation and electrochemical performance of α-MnO2 electrode material for aqueous zinc ion battery. Chinese Journal of Inorganic Chemistry, 2026, 42(3): 479-487. doi: 10.11862/CJIC.20250292

    4. [4]

      Ruiying Liu ,  Li Zhao ,  Baishan Liu ,  Jiayuan Yu ,  Yujie Wang ,  Wanqiang Yu ,  Di Xin ,  Chaoqiong Fang ,  Xuchuan Jiang ,  Riming Hu ,  Hong Liu ,  Weijia Zhou . Modulating pollutant adsorption and peroxymonosulfate activation sites on Co3O4@N,O doped-carbon shell for boosting catalytic degradation activity. Chinese Journal of Structural Chemistry, 2024, 43(8): 100332-100332. doi: 10.1016/j.cjsc.2024.100332

    5. [5]

      Sanmei Wang , Dengxin Yan , Wenhua Zhang , Liangbing Wang . Graphene-supported isolated platinum atoms and platinum dimers for CO2 hydrogenation: Catalytic activity and selectivity variations. Chinese Chemical Letters, 2025, 36(4): 110611-. doi: 10.1016/j.cclet.2024.110611

    6. [6]

      Guoping Yang , Zhoufu Lin , Xize Zhang , Jiawei Cao , Xuejiao Chen , Yufeng Liu , Xiaoling Lin , Ke Li . Assembly of Y(Ⅲ)-containing antimonotungstates induced by malic acid with catalytic activity for the synthesis of imidazoles. Chinese Chemical Letters, 2024, 35(12): 110274-. doi: 10.1016/j.cclet.2024.110274

    7. [7]

      Qing Li , Bing Wang , Qi Xu , Ruiyou Liu , Chen Li , Fang Luo , Yifei Li , Yingjie Yu , Zehui Yang . Pt dopants in ruthenium/iridium oxides promote catalytic activity in overall acidic water splitting. Chinese Chemical Letters, 2025, 36(12): 111658-. doi: 10.1016/j.cclet.2025.111658

    8. [8]

      Ruhe Zhang , Dandan Li , Ting Liang , Xinyu Zhang , Jingyi Hou , Yang Kang , Dongjun Lin , Jun Wu . Dual redox-responsive CO2-generating nanoparticles assembled from one-step synthesized L-cystine-based biodegradable polymers for enhanced chemotherapy of tumors. Chinese Chemical Letters, 2026, 37(7): 111680-. doi: 10.1016/j.cclet.2025.111680

    9. [9]

      Jianyun Li , Lifei Zou , Jianwei Cao , Zhaohui Shi , Zhiwei Liu , Lirong Zhang , Jiyang Li , Xin Liu , Yunling Liu . A unique two-fold interpenetrated zeolite-like metal–organic framework with SOD topology for one-step C2H4 purification from ternary mixtures. Chinese Chemical Letters, 2026, 37(8): 111189-. doi: 10.1016/j.cclet.2025.111189

    10. [10]

      Yunli Xu , Xuwen Da , Lei Wang , Yatong Peng , Wanpeng Zhou , Xiulian Liu , Yao Wu , Wentao Wang , Xuesong Wang , Qianxiong Zhou . Ru(Ⅱ)-based aggregation-induced emission (AIE) agents with efficient 1O2 generation, photo-catalytic NADH oxidation and anticancer activity. Chinese Chemical Letters, 2025, 36(5): 110168-. doi: 10.1016/j.cclet.2024.110168

    11. [11]

      Zhou Li ,  Mengxue Yu ,  Shixin Chang ,  Zhibin Huang ,  Zhenmin Cheng ,  Weibin Zhang ,  Sónia A. C. Carabineiro ,  Zhigao Xu ,  Kangle Lv . Enhancing the photocatalytic activity of crystalline g-C3N4 towards NO oxidation and CO2 reduction through K+-doping and cyano defect engineering. Chinese Journal of Structural Chemistry, 2026, 45(1): 100698-100698. doi: 10.1016/j.cjsc.2025.100698

    12. [12]

      Lanfang Wang , Jiangnan Lv , Yujia Li , Yanqing Hao , Wenjiao Liu , Hui Zhang , Xiaohong Xu . One-step synthesis of nanowoven ball-like NiS-WS2 for high-efficiency hydrogen evolution. Chinese Chemical Letters, 2025, 36(1): 109597-. doi: 10.1016/j.cclet.2024.109597

    13. [13]

      Xian XIA , Qin SHI , Wanyi SU , Qingjun XUE , Honghui PAN , Xixiang LIU , Chuanqi ZHAO . In-situ synthesis of Bi2O3@BiVO4 composite via solvothermal method and its adsorption performance for rhodamine B in water. Chinese Journal of Inorganic Chemistry, 2026, 42(5): 1096-1112. doi: 10.11862/CJIC.20250311

    14. [14]

      Lijun Liao , Yuhao Wang , Yanbo Li , Yingchun Chen , Ruting Yuan , Bo Wang , Tiancheng Zhuang , Guangquan Zhao , Wei Zhou . Synergy of electron-trapping centers and solid adsorption toward 100% suppression of toxic byproduct N2O in photocatalytic NO reduction. Chinese Chemical Letters, 2026, 37(3): 111398-. doi: 10.1016/j.cclet.2025.111398

    15. [15]

      Anqiu LIU , Long LIN , Dezhi ZHANG , Junyu LEI , Kefeng WANG , Wei ZHANG , Junpeng ZHUANG , Haijun HAO . Synthesis, structures, and catalytic activity of aluminum and zinc complexes chelated by 2-((2,6-dimethylphenyl)amino)ethanolate. Chinese Journal of Inorganic Chemistry, 2024, 40(4): 791-798. doi: 10.11862/CJIC.20230424

    16. [16]

      Qinwen Zheng , Xin Liu , Lintao Tian , Yi Zhou , Libing Liao , Guocheng Lv . Mechanism of Fenton catalytic degradation of Rhodamine B induced by microwave and Fe3O4. Chinese Chemical Letters, 2025, 36(4): 109771-. doi: 10.1016/j.cclet.2024.109771

    17. [17]

      Fei ZHOU , Xiaolin JIA . Co3O4/TiO2 composite photocatalyst: Preparation and synergistic degradation performance of toluene. Chinese Journal of Inorganic Chemistry, 2024, 40(11): 2232-2240. doi: 10.11862/CJIC.20240236

    18. [18]

      Tao Tang , Chen Li , Sipu Li , Zhong Qiu , Tianqi Yang , Beirong Ye , Shaojun Shi , Chunyang Wu , Feng Cao , Xinhui Xia , Minghua Chen , Xinqi Liang , Xinping He , Xin Liu , Yongqi Zhang . One-step constructing advanced N-doped carbon@metal nitride as ultra-stable electrocatalysts via urea plasma under room temperature. Chinese Chemical Letters, 2024, 35(11): 109887-. doi: 10.1016/j.cclet.2024.109887

    19. [19]

      Jinyu Li , Junlei Wang , Shilong Li , Kun Wang . One-step preparation of Mg/Mo co-doped cobalt-free nickel-rich cathode materials with high capacity and long cycle through flame-assisted spray pyrolysis. Chinese Chemical Letters, 2026, 37(11): 111855-. doi: 10.1016/j.cclet.2025.111855

    20. [20]

      Doudou Bao , Jinwei Zhou , Ayaz , Li Wang , Xiangming He , Ziang Jiang , Feixiang Wu . Enhancing cycling stability of high-nickel cobalt-free LiNiO2 through La/Al synergistic modification: A one-step synthesis approach. Chinese Chemical Letters, 2026, 37(11): 111774-. doi: 10.1016/j.cclet.2025.111774

Metrics
  • PDF Downloads(11)
  • Abstract views(1517)
  • HTML views(199)

通讯作者: 陈斌, bchen63@163.com
  • 1. 

    沈阳化工大学材料科学与工程学院 沈阳 110142

  1. 本站搜索
  2. 百度学术搜索
  3. 万方数据库搜索
  4. CNKI搜索
Address:Zhongguancun North First Street 2,100190 Beijing, PR China Tel: +86-010-82449177-888
Powered By info@rhhz.net

/

DownLoad:  Full-Size Img  PowerPoint
Return