Citation: Hu Ziqiao, Liu Sihai, Liu Jinhua, Li Xiuyun. Progress in Thermal Stability of Water-Soluble Polymers[J]. Chemistry, ;2016, 79(8): 714-718,722. shu

Progress in Thermal Stability of Water-Soluble Polymers

  • Corresponding author: Hu Ziqiao, 
  • Received Date: 5 April 2016
    Available Online: 26 April 2016

    Fund Project:

  • Water-soluble polymers are widely used in petroleum development, water treatment, paper making, printing, medicine and so on, whose application at high temperature depends on their thermal stability. In this paper, the thermal performances of several typical water-soluble polymers are reviewed. Furthermore, the mechanisms of thermal degradation for different types of water-soluble polymers are revealed. In addition, the effect of molecular structure and external additives on thermal stability is discussed as well. Finally, the development prospects of water-soluble polymers utilized in high temperature environment are explored.
  • 加载中
    1. [1]

      [1] 严瑞瑄. 水溶性高分子. 北京: 化学工业出版社, 1998:105~106.

    2. [2]

      [2] 王中华. 石油钻探技术, 2009, 37(3): 1~7.

    3. [3]

      [3] 辛军, 郭建春, 赵金洲等. 钻井液与完井液, 2009, 26(6): 49~52.

    4. [4]

      [4] 蒋婵杰, 潘春跃, 黄可龙. 高分子通报, 2001, (3): 64~69.

    5. [5]

      [5] D A Z Wever, F Picchioni, A A Broekhuis. Prog. Polym. Sci., 2011, 36(11): 1558~1628.

    6. [6]

      [6] D ChunStandnes, I Skjevrak. J. Petrol. Sci. Eng., 2014, 122: 761~775.

    7. [7]

      [7] W M Leung, D E Axelson, J D van Dyke. J. Polym. Sci. Part A, Polym. Chem., 1987, 25(7): 1825~1846.

    8. [8]

      [8] M H Yang. Polym. Test., 1998, 17(3): 191~198.

    9. [9]

      [9] S Mukherjee, M H Mondal, M Mukherjee et al. Macromolecules, 2009, 42(20): 7889~7896.

    10. [10]

      [10] Y A Aggour. Polym. Degrad. Stab., 1994, 44(1): 71~73.

    11. [11]

      [11] L L Xu, L X Che, J Zheng et al. RSC Adv., 2014, 4(63): 33269~33278.

    12. [12]

      [12] M Silva, E R Dutra, V Mano et al. Polym. Degrad. STab., 2000, 67(3): 491~495.

    13. [13]

      [13] C D Vlad, M V Dinu, S Dragan. Polym. Degrad. Stab., 2003, 79(1): 153~159.

    14. [14]

      [14] N B Shukla, G Madras. J. Appl. Polym. Sci., 2012, 125(1): 630~639.

    15. [15]

      [15] R G Sousa, W F Magalhaes, R F S Freitas. Polym. Degrad. Stab., 1998, 61(2): 275~281.

    16. [16]

      [16] M H Yang. Polym. Test., 2000, 19(1): 85~91.

    17. [17]

      [17] N Limparyoon, N Seetapan, S Kiatkamjornwong. Polym. Degrad. Stab., 2011, 96(6): 1054~1063.

    18. [18]

      [18] S Shin, Y I Cho. KSME Int. J., 1998, 12(2):267~273.

    19. [19]

      [19] V F Kurenkov, P V Trofimov, A V Kurenkov et al. Russ. J. Appl. Chem., 2005, 78(78): 995~999.

    20. [20]

      [20] B I Choi, M S Jeong, K S Lee. Polym. Degrad. Stab., 2014, 110: 225~231.

    21. [21]

      [21] H Kheradmand, J Francois, V Plazanet. Polymer, 1988, 29(5): 860~870.

    22. [22]

      [22] Q Ma, P J Shuler, C W Aften et al. Polym. Degrad. Stab., 2015, 121: 69~77.

    23. [23]

      [23] W O Parker Jr, A Lezzi. Polymer, 1993, 34(23): 4913~4918.

    24. [24]

      [24] J Cao, Y Tan, Y Che et al. J. Polym. Res., 2011, 18(2): 171~178.

    25. [25]

      [25] M C Mcgaugh, S Kottle. J. Polym. Sci. Part B: Polym. Lett., 1967, 5(9): 817~820.

    26. [26]

      [26] A Eisenberg, T Yokoyama, E Sambalido. J. Polym. Sci. Part A: Polym. Chem., 1969, 7(7): 1717~1728.

    27. [27]

      [27] F X Roux, R Audebert, C Quivoron. Eur. Polym. J., 1973, 9(8): 815~825.

    28. [28]

      [28] A Gurkaynak, F Tubert, J Yang et al. J. Polym. Sci. Part A: Polym. Chem., 1996, 34(3): 349~355.

    29. [29]

      [29] L Lepine, R Gilbert. Polym. Degrad. Stab., 2002, 75(2): 337~345.

    30. [30]

      [30] N B Shukla, N Daraboina, G Madras. Polym. Degrad. Stab., 2009, 94(8): 1238~1244.

    31. [31]

      [31] Y Huang, J Lu, C Xiao. Polym. Degrad. Stab., 2007, 92(6): 1072~1081.

    32. [32]

      [32] N P Bayramgil. Polym. Degrad. Stab., 2008, 93(8): 1504~1509.

    33. [33]

      [33] L Ruiz-Rubio, J L Vilas, M Rodriguez et al. Polym. Degrad. Stab., 2014, 109:147~153.

    34. [34]

      [34] S Dubinsky, G S Grader, G E Shter et al. Polym. Degrad. Stab., 2004, 86(1): 171~178.

    35. [35]

      [35] 江献财, 董海亚, 谢静思等. 高分子通报, 2010, (10): 38~45.

    36. [36]

      [36] B J Holland, J N Hay. Polymer, 2001, 42(16): 6775~6783.

    37. [37]

      [37] P Thomas, J P Guerbois, G Russell et al. J. Therm. Anal. Calorim., 2001, 64(2): 501~508.

    38. [38]

      [38] P Zheng, X K Ling. Polym. Degrad. Stab., 2007, 92: 1061~1071.

    39. [39]

      [39] A Uda, S Morita, Y Ozaki. Polymer, 2013, 54(8): 2130~2137.

    40. [40]

      [40] H Kaczmarek, A Podgorski. Polym. Degrad. Stab., 2007, 92(6): 939~946.

    41. [41]

      [41] H Lu, C A Wilkie, M Ding et al. Polym. Degrad. Stab., 2011, 96(5): 885~891.

    42. [42]

      [42] L Dulog, G Storck. Makromol. Chem., 1966, 91(1):50~73.

    43. [43]

      [43] J Glastrup. Polym. Degrad. Stab., 1996, 52(3): 217~222.

    44. [44]

      [44] L Yang, F Heatley, T G Blease. Eur. Polym. J., 1996, 32(5): 535~547.

    45. [45]

      [45] O A Mkhatresh, F Heatley. Macromol. Chem. Phys., 2002, 203(16): 2273~2280.

    46. [46]

      [46] G Gallet, S Carroccio, P Rizzarelli et al. Polymer, 2002, 43: 1081~1094.

    47. [47]

      [47] K Gjurova, C Uzov, A Popov et al. J. Appl. Polym. Sci., 1999, 74(14): 3324~3330.

  • 加载中
    1. [1]

      Xuewei BACheng CHENGHuaikang ZHANGDeqing ZHANGShuhua LI . Preparation and luminescent performance of Sr1-xZrSi2O7xDy3+ phosphor with high thermal stability. Chinese Journal of Inorganic Chemistry, 2025, 41(2): 357-364. doi: 10.11862/CJIC.20240096

    2. [2]

      Tong WANGXuefang ZHUQi GAOHongbo ZHANGChao RENLixia GE . Luminescence and thermal stability of Tb3+-Eu3+ doped glass-ceramics containing Na8.12Y1.293Si6O18 crystal phase. Chinese Journal of Inorganic Chemistry, 2025, 41(11): 2237-2250. doi: 10.11862/CJIC.20250137

    3. [3]

      Yuchen ZhouHuanmin LiuHongxing LiXinyu SongYonghua TangPeng Zhou . Designing thermodynamically stable noble metal single-atom photocatalysts for highly efficient non-oxidative conversion of ethanol into high-purity hydrogen and value-added acetaldehyde. Acta Physico-Chimica Sinica, 2025, 41(6): 100067-0. doi: 10.1016/j.actphy.2025.100067

    4. [4]

      Xiqing Liang Tian Zhao Jiawei Li Haohui Tan Hai Chen Liyan Zeng . Pentaerythritol’s Journey of Making Friends. University Chemistry, 2025, 40(10): 175-185. doi: 10.12461/PKU.DXHX202412009

    5. [5]

      Zeyi Yan Ruitao Liu Xinyu Qi Yuxiang Zhang Lulu Sun Xiangyuan Li Anchao Feng . Exploration of Suspension Polymerization: Preparation and Fluorescence Stability of Perovskite Polystyrene Microbeads. University Chemistry, 2025, 40(4): 72-79. doi: 10.12461/PKU.DXHX202405110

    6. [6]

      Wang WangYucheng LiuShengli Chen . Use of NiFe Layered Double Hydroxide as Electrocatalyst in Oxygen Evolution Reaction: Catalytic Mechanisms, Electrode Design, and Durability. Acta Physico-Chimica Sinica, 2024, 40(2): 2303059-0. doi: 10.3866/PKU.WHXB202303059

    7. [7]

      Xinyi MAYuhang XIAOQian LIZihuan YANChengyan LIUXiguang GAOHongju YINFeixiang CHENG . Thienyl metal coordination polymers: Preparation and photocatalytic degradation performance of phenol. Chinese Journal of Inorganic Chemistry, 2026, 42(5): 969-979. doi: 10.11862/CJIC.20250317

    8. [8]

      Shitao Fu Jianming Zhang Cancan Cao Zhihui Wang Chaoran Qin Jian Zhang Hui Xiong . Study on the Stability of Purple Cabbage Pigment. University Chemistry, 2024, 39(4): 367-372. doi: 10.3866/PKU.DXHX202401059

    9. [9]

      Jinyang SUIZhonghao NIUHao XUJingli XIE . Zinc(Ⅱ) coordination polymers from mixed triazole and carboxylate ligands: Synthesis and properties for CO2 cycloaddition and photocatalytic dye degradation. Chinese Journal of Inorganic Chemistry, 2026, 42(8): 1603-1612. doi: 10.11862/CJIC.20260089

    10. [10]

      Dongdong Yao JunweiGu Yi Yan Junliang Zhang Yaping Zheng . Teaching Phase Separation Mechanism in Polymer Blends Using Process Representation Teaching Method: A Teaching Design for Challenging Theoretical Concepts in “Polymer Structure and Properties” Course. University Chemistry, 2025, 40(4): 131-137. doi: 10.12461/PKU.DXHX202408125

    11. [11]

      Xuyang Wang Jiapei Zhang Lirui Zhao Xiaowen Xu Guizheng Zou Bin Zhang . Theoretical Study on the Structure and Stability of Copper-Ammonia Coordination Ions. University Chemistry, 2024, 39(3): 384-389. doi: 10.3866/PKU.DXHX202309065

    12. [12]

      Xiaoning TANGJunnan LIUXingfu YANGJie LEIQiuyang LUOShu XIAAn XUE . Effect of sodium alginate-sodium carboxymethylcellulose gel layer on the stability of Zn anodes. Chinese Journal of Inorganic Chemistry, 2024, 40(8): 1452-1460. doi: 10.11862/CJIC.20240191

    13. [13]

      Yingtong ShiGuotong XuGuizeng LiangDi LanSiyuan ZhangYanru WangDaohao LiGuanglei Wu . PEG-VN改性PP隔膜用于高稳定性高效率锂硫电池. Acta Physico-Chimica Sinica, 2025, 41(7): 100082-0. doi: 10.1016/j.actphy.2025.100082

    14. [14]

      Xiaojing TianZhichun HuangQingsong ZhangXu WangNing YangNanping Deng . PNIPAm Thermo-Responsive Nanofibers Mats: Morphological Stability and Response Behavior under Cross-Linking. Acta Physico-Chimica Sinica, 2024, 40(4): 2304037-0. doi: 10.3866/PKU.WHXB202304037

    15. [15]

      Yawen GuoDawei LiYang GaoCuihong Li . Recent Progress on Stability of Organic Solar Cells Based on Non-Fullerene Acceptors. Acta Physico-Chimica Sinica, 2024, 40(6): 2306050-0. doi: 10.3866/PKU.WHXB202306050

    16. [16]

      Haihuan YUJing SUNZhongmin SU . Research progress of water-stable metal-organic frameworks fluorescent sensors in food safety detection. Chinese Journal of Inorganic Chemistry, 2026, 42(8): 1569-1581. doi: 10.11862/CJIC.20260062

    17. [17]

      Yahui HANJinjin ZHAONing RENJianjun ZHANG . Synthesis, crystal structure, thermal decomposition mechanism, and fluorescence properties of benzoic acid and 4-hydroxy-2, 2′: 6′, 2″-terpyridine lanthanide complexes. Chinese Journal of Inorganic Chemistry, 2025, 41(5): 969-982. doi: 10.11862/CJIC.20240395

    18. [18]

      Jiaxi Xu Yuan Ma . Influence of Hyperconjugation on the Stability and Stable Conformation of Ethane, Hydrazine, and Hydrogen Peroxide. University Chemistry, 2024, 39(11): 374-377. doi: 10.3866/PKU.DXHX202402049

    19. [19]

      Yuxia Luo Xiaoyu Xie Fangfang Chen . 药物递送魔法师——分子印迹聚合物. University Chemistry, 2025, 40(8): 202-210. doi: 10.12461/PKU.DXHX202409129

    20. [20]

      Jing SUBingrong LIYiyan BAIWenjuan JIHaiying YANGZhefeng Fan . Highly sensitive electrochemical dopamine sensor based on a highly stable In-based metal-organic framework with amino-enriched pores. Chinese Journal of Inorganic Chemistry, 2024, 40(7): 1337-1346. doi: 10.11862/CJIC.20230414

Metrics
  • PDF Downloads(0)
  • Abstract views(1143)
  • HTML views(150)

通讯作者: 陈斌, bchen63@163.com
  • 1. 

    沈阳化工大学材料科学与工程学院 沈阳 110142

  1. 本站搜索
  2. 百度学术搜索
  3. 万方数据库搜索
  4. CNKI搜索
Address:Zhongguancun North First Street 2,100190 Beijing, PR China Tel: +86-010-82449177-888
Powered By info@rhhz.net

/

DownLoad:  Full-Size Img  PowerPoint
Return